RC Series Dead Weight Creep & Rupture Testing Machine

2024-12-25 15:14 alreadyPeople browse 小编

ClassificationCreep Testing Machine

productRC Series Dead Weight Creep & Rupture Testing Machine

size

length

price

Phone 13969111546

Applications:This testing machine is designed and built for testing the creep pr...

Details

Applications:

This testing machine is designed and built for testing the creep properties and creep rupture strength on ferrous metal, nonferrous metal and their alloy that subjects to constant tensile load at a certain temperature at the specified time interval. It is designed according to “ high temperature creep & rupture strength GB/2039-1997” National Standard. Meanwhile, it conforms to ISO204/1997 International Standard and HB5151-96 Aviation Industrial Standard. It can offer liable test/inspection certificate for aviation Industry & other special materials property that should endure high temperature.

 

Specification:

Capacity: Model RC-30: 30KN; Model RC-50: 50KN; Model RC-100: 100KN; Model RC-200: 200KN

Load range: 2-100% FS

Load accuracy: ≤±1.0%

Variation of indicating load value: ≤±1.0%

The eccentricity of the upper and lower chucks: ≤10%

Min dead weight load: 1N

Automatic level range: ±0.1mm

Lever ratio: 1:50 / 1:100

Lower tensile rod speed: 0-50mm/min

Lower tensile rod stroke: 0-150mm for RC-30 and RC-50; 0-200mm for RC-100 and RC-200

 

High temperature furnace & Temperature-controller

l Working Temp. range: 400℃~1200℃

l Length of effective soaking zone: 150mm

l Furnace pipe & electric furnace size:

Furnace pipe: φ90mm (Inner Dia.)×400mm (L),

Furnace: φ300mm (outer Dia,)×420mm (L);

Furnace life: ≥3000hours (Constant working time less than 1000℃)

l Furnace Temperature accuracy (℃):

Test Temperature

Temperature fluctuation

Temperature gradient

≤600

±2

2

>600~900

±3

3

>900~1200

±4

4

l Measure & Control temperature meter: digital display, sensitivity: 0.1℃;

l Auto compensation error of cold end:≤0.5℃;

l To be matched freely with thermocouple.

l Moving speed of lower grip holder

Speed range: 0.005~50mm/min;

Error: ±0.5%

l Timing error: ±0.2%


Deformation measurement

l Gauge length: 50mm (or 100mm);

l Max. Deformation: 5mm (or 10mm)

l Resolution: 0.001mm

l Error: 0.002mm